节点文献
铜及铜合金在淡海水交替自然环境条件下的腐蚀行为研究
Corrosion Behavior of Copper and Its Alloys in Freshwater-Seawater Alternate Circumstance
【摘要】 目的研究铜及铜合金在淡海水交替条件下的腐蚀行为。方法通过开展TUP纯铜、B10与B30铜合金3种典型的铜及铜合金在淡海水交替、海水及淡水自然环境下2年的暴露试验,将三种环境下材料的腐蚀形貌、腐蚀速率进行对比,总结3种材料在不同水环境下的腐蚀规律,对其腐蚀机理进行简要的探讨,并对其长周期的腐蚀行为进行预测。结果对TUP纯铜来说,淡海水环境对TUP纯铜的影响是海水环境的1.66倍,对B30铜合金来说,淡海水环境对其影响是海水环境的2.07倍,而对于B10铜合金,淡海水环境是海水环境的2.17倍。结论从耐蚀性上来看,铜及合金在淡海水交替自然环境下耐蚀性能最差,海水自然环境下次之,在淡水环境下的耐蚀性能最好,自然环境中水的流速越快,会加重铜及合金的腐蚀。
【Abstract】 Objective To study corrosion behaviors of copper and its alloys in seawater-freshwater alternate circumstance. Methods Three kinds of typical metals, including Tup pure copper, B10 and B30 copper alloys, were exposed in seawater, freshwater and seawater/freshwater alternate circumstance for 2 years to compare the data of corrosion morphology and corrosion rate. The corrosion rules of 3 kinds of metals in different water circumstances were summarized, the corrosion mechanism were discussed, and the long-term corrosion behaviors were also predicted. Results Influences of seawater-freshwater alternate circumstance on Tup pure copper was 1.66 times of that of seawater. Influences of seawater-freshwater alternate circumstance on B30 copper alloy was 2.07 times of that of seawater. Influences of seawater-freshwater alternate circumstance on B10 copper alloy was 2.17 times of that of seawater. Conclusion Sequence of copper and its alloys corrosion resistance is fresh water, seawater and seawater-freshwater alternate circumstance. The corrosion of copper and its alloys are more serious under higher flow velocity of water in natural environment.
【Key words】 copper; copper alloy; corrosion; flow velocity; seawater-freshwater alternate circumstance;
- 【文献出处】 装备环境工程 ,Equipment Environmental Engineering , 编辑部邮箱 ,2017年02期
- 【分类号】TG172.5
- 【被引频次】12
- 【下载频次】468