Modification Effects on Poly( lactic acid ) by Nano-Size PolymethylsiloxanePoly( methy-methacrylate) core / Shell Spheres
【摘要】 采用种子乳液聚合方法制备了纳米软核/硬壳聚甲基硅氧烷/聚甲基丙烯酸甲酯粒子,并将其应用于聚乳酸PLA改性。对所得复合材料的拉伸强度、分散性、结晶性等性能进行了测试。结果表明:软核/硬壳聚甲基硅氧烷/聚甲基丙烯酸甲酯粒子在聚乳酸基体中分散良好,能作为成核剂诱导聚乳酸结晶,还能增加聚乳酸的拉伸强度。当添加量为3%时,聚乳酸复合材料的的拉伸强度达到79.33 MPa,结晶度达到37.26%;而相同条件下,纯聚乳酸的拉伸强度仅为65.45 MPa,结晶度仅为0.01%。
【Abstract】 Using seed emulsion polymerization method,polymethylsiloxane-poly( methy-methacrylate) core / shell spheres was perpetrated,using it as filler,poly( lactic acid) was modified. The tensile strength,dispersibility,crystallization were tested. The result showed that nano-size polymethylsiloxane-poly( methy-methacrylate) core / shell spheres dispersed well and acted as a nucleating agent in PLA,the tensile strength of PLA was also improved. When the addition amount reached 3%,the tensile strength of the composite material reached 79. 33 MPa,the degree of crystallinity reached 37. 26%. While the tensile strength of pure poly( lactic acid) was only 65. 45 MPa,the degree of crystallinity was only 0. 01%.
【Key words】 core / shell; polymethylsiloxane; poly(lactic-acid); enhance; crystallization;
- 【文献出处】 塑料 ,Plastics , 编辑部邮箱 ,2015年01期
- 【分类号】TQ323.4
- 【被引频次】7
- 【下载频次】243