节点文献

W-plug via electromigration in CMOS process

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 赵文彬; 陈海峰; 肖志强; 李蕾蕾; 于宗光;

【Author】 Zhao Wenbin1,2,Chen Haifeng2,Xiao Zhiqiang2,Li Leilei1,and Yu Zongguang1,2(1 School of Microelectronics,Xidian University,Xi’an 710071,China)(2 No.58 Institute,China Electronic Technology Group Corporation,Wuxi 214035,China)

【机构】 School of Microelectronics,Xidian University; No.58 Institute,China Electronic Technology Group Corporation;

【摘要】 We analyze the failure mechanism of W-plug via electromigration made in a 0.5-μm CMOS SPTM process.Failure occurs at the top or bottom of a W-plug via.We design a series of via chains,whose size ranges from 0.35 to 0.55μm.The structure for the via electromigration test is a long via chain,and the layer in the via is Ti/TiN/W/TiN.Using a self-heated resistor to raise the temperature of the via chain allows the structure to be stressed at lower current densities,which does not cause significant joule heating in the plugs.This reduces the interaction between the plug and the plug contact resistance and the time-to-failure for the via chain.The lifetime of a W-plug via electromigration is on the order of 3×107s,i.e.,far below the lifetime of metal electromigration.The study on W-plug via electromigraion in this paper is beneficial for wafer level reliability monitoring of the ultra-deep submicron CMOS multilayer metal interconnect process.

【Abstract】 We analyze the failure mechanism of W-plug via electromigration made in a 0.5-μm CMOS SPTM process.Failure occurs at the top or bottom of a W-plug via.We design a series of via chains,whose size ranges from 0.35 to 0.55μm.The structure for the via electromigration test is a long via chain,and the layer in the via is Ti/TiN/W/TiN.Using a self-heated resistor to raise the temperature of the via chain allows the structure to be stressed at lower current densities,which does not cause significant joule heating in the plugs.This reduces the interaction between the plug and the plug contact resistance and the time-to-failure for the via chain.The lifetime of a W-plug via electromigration is on the order of 3×107s,i.e.,far below the lifetime of metal electromigration.The study on W-plug via electromigraion in this paper is beneficial for wafer level reliability monitoring of the ultra-deep submicron CMOS multilayer metal interconnect process.

【关键词】 W-plug; self-heated; electromigration; lifetime;
【Key words】 W-plug; self-heated; electromigration; lifetime;
【基金】 supported by the Series Program for Electronic Component and Device Spectrum
  • 【文献出处】 半导体学报 ,Journal of Semiconductors , 编辑部邮箱 ,2009年05期
  • 【分类号】TN432
  • 【下载频次】41
节点文献中: