节点文献

涟钢130m~2烧结机的技术改造

MODIFICATION OF 130 m~2 SINTERING PLANT IN LIANYUAN I&S CO.

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【摘要】 针对涟钢 13 0m2 烧结机混合料水分波动大 ,布料操作困难 ,影响生产稳定的问题 ,进行了相应改造。主要包括 :增设红外线测水系统、采用宽皮带 -九辊布料、二混蒸汽预热系统改造、综合利用炼钢污泥等。改造后 ,生产过程稳定 ,烧结矿产质量提高 ,取得了显著的经济效益

【Abstract】 Point at some problems,e g the fluctuation of mix moisture content is larger,the mix feeding is difficult and the sintering operating is not smooth etc ,the 130?m 2 sintering plant in Lianyuan I&S Co was modified in the year 2001 With adoption of the infrared moisture measuring device and the wide belt-nine rollers feeder and complex utilization of the ironmaking mud,the sintering operation was smoothed, the productivity was increased,the sinter quality was improved and the obvious benefit was obtained

【关键词】 烧结机技术改造综合利用
【Key words】 sintering plantmodificationcomplex utilization
  • 【文献出处】 烧结球团 ,Sintering and Pelletizing , 编辑部邮箱 ,2004年01期
  • 【分类号】TF321
  • 【被引频次】4
  • 【下载频次】74