红色Y2O2S:Eu3+磷光材料的沉淀法制备和发光性能研究
Preparation and Characterization of Y2O2S:Eu3+ Phosphors by Co-precipitation Method
【摘要】 用沉淀法制备了Eu3+掺杂的Y2O2S磷光材料,测量并研究了掺杂不同物质的量的Eu3+离子的Y2O2S磷光材料的发射谱和激发谱.发射光谱对应了Eu3+离子5DJ(J=0,1,2,3)-7FJ(J=0,1,2,3,4)的特征发射,激发光谱主峰对应260,345,468,540nm等,余辉时间(到人眼的最小亮度分辨率0.32mcd/m2)可达1h以上.
【Abstract】 Synthesis of the Eu3+-activated Y2O2S by Co-precipitation method was presented. The crystalline phases by direct sintering method and Co-precipitation method were investigated. The excitation spectra and emission spectra of Y2O2S phosphors doped with different Eu3+ molar ratio were measured. The main emission peaks ascribed to Eu3+ ions transition from ()5DJ(J=0,1.2)to ()7FJ(J=0,1,2,3,4) were found. The main excitation peaks includes 260 nm, 345 nm, 468 nm, 540 nm etc. The afterglow time was over 1 hour in the light perception of the dark-adapted human eye (0.32 mcd/m2).
- 【文献出处】 河北大学学报(自然科学版) ,Journal of Hebei University(Natural Science Edition) , 编辑部邮箱 ,2004年06期
- 【分类号】O482.31
- 【被引频次】16
- 【下载频次】227