节点文献
水平连铸QSn6.5-0.1带坯冷轧开裂问题的初步探讨
Preliminary Analysis of Cause of Cracks in QSn6.5-0.1 Strip Produced by Horizontal Continuous Casting
【摘要】 对水平连铸QSn6 5 0 1带坯在冷轧过程中出现的开裂现象进行了检验和初步分析 ,结果表明 :带坯下表面出现微小裂纹 ,在卷取、轧制的反复拉应力作用下导致表面开裂 ;内部线状、蚯蚓状裂纹是由显微缩松逐步演变而来。
【Abstract】 s:The cracks in the captioned strip in cold rolling are tested and preliminarily analyzed with the results showing that the fine cracks in the lower surface of the cast strip leads to the cracks in the strip during coiling ard rolling due to repeated action of drawing stresses and that the internal cracks like earthworms have gradually evolved from microporosity.
【关键词】 水平连铸;
QSn6501;
冷轧;
裂纹;
应力;
显微缩松;
【Key words】 horizontal continuous casting; QSn6 5 0 1; cold rolling; cracks; stress; microporosity;
【Key words】 horizontal continuous casting; QSn6 5 0 1; cold rolling; cracks; stress; microporosity;
- 【文献出处】 上海有色金属 ,Shanghai Nonferrous Metals , 编辑部邮箱 ,2002年02期
- 【分类号】TG335.12
- 【被引频次】2
- 【下载频次】109