节点文献
308L和347L焊缝金属的氢致滞后断裂行为
Hydrogen Induced Delayed Fracture of 308L and 347L Weld Metal
【摘要】 奥氏体不锈钢 30 8L和 347L的焊缝金属能发生氢致滞后断裂 ,而且比 30 4L母材更敏感。用单边缺口试样动态充氢法测出的氢致滞后断裂门槛应力强度因子 KIH随可扩散氢浓度 C0 的对数而线性下降。 3种材料氢致滞后断口的形貌与 KI 以及 C0 有关 ,当 KI 较高或 C0 较小时是韧窝断口 ;当 KI 较低或 C0 较高时是脆性断口
【Abstract】 It has been found that hydrogen induced delayed fracture could occur in 308L and 347L weld metal, and the threshold stress intensity for 308L and 347L is lower than 304L austenitic stainless steel. For single edge notched specimen which is dynamically charged hydrogen under load, the threshold stress intensity K IH for 308L, 347L and 304L decreases with the increase of the diffusible hydrogen content C 0. The mode of hydrogen induced delayed fracture in the three materials is correlated with the K I and C 0 value.
【Key words】 austenitic stainless steel; weld metal; hydrogen-induced delayed fracture;
- 【文献出处】 钢铁研究学报 ,JOURNAL OF IRON AND STEEL RESEARCH , 编辑部邮箱 ,2000年S1期
- 【分类号】TG44
- 【被引频次】1
- 【下载频次】145