断裂力学在转化管剩余寿命预测中的应用

Application of Fracture Mechanics to Prediction of Residual Life of Reformer Tube

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 朱世杰李雪辉徐善国王富岗

【Author】 Zhu Shijie, Li Xuehui, Xu Shanguo, Wang Fugang (Dept. of Materials Engineering, DUT)

【机构】 大连理工大学材料工程系大连理工大学材料工程系

【摘要】 在830~1000°C温度和3.3~7.8 MPam初始应力强度因子下研究了运 行81 000 h的HK 40转化管的蠕变裂纹扩展行为,由裂纹扩展速率与温度的Arrhenius 关系和裂纹扩展速率与断裂时间的反比关系导出Larson-Miller参数(P),从而建立 了初始应力强度因子(Krr)和 Larson-Miller参数关系外推寿命的方法.

【Abstract】 The creep crack growth behavior of HK40 reformer tube that has serviced for 81 000 hours has been studied in the temperature range of 830 to 1 000 C and in the initial stress intensity factor range of 3.3 to 7.8 MP.am1/2. According to the Arrhenius relation of crack growth rate with temperature and the inversely proportional relation of crack growth rate with rupture time, Larson-Miller parameter is derived. A method ext-roplating residual life by the relation of initial stress intensity factor with Larson-Miller parameter(P) is propose.

【关键词】 断裂力学蠕变裂纹寿命/转化管
【Key words】 fracture mechanicscreepcrackslife/reformer tube