Various processes of making high titanium ferroalloy(Ti>65%) by reducing ilmenite were investigated in the article,with the thermite method being focused on.The thermite method was performed in a laboratory condition,in which the main factors affecting titanium recovery rate were investigated.It was found possible to make high titanium ferroalloy with thermite method,though the impurity level was rather difficult to be controlled in the process.