The objective of this study was to evaluate possible changes of a new-type dental CAD/CAM machinable glass-ceramic in a provocative corrosive environment according to ISO 6872. After contacted with the corrosive environment, observed by SEM, the exposed surface was covered in fewer voids in the part of glass phase, which is similar to other dental ceramics. These voids initiate damage while loading, thus the strength decreased.