The ratio Q/W of heat energy to total electricity energy in microarc oxidation of aluminum alloys is determined by calorimetry. This ratio changes between 50% and 80%, it increases with increase in solution concentration. Otherwise, the ratio of pure aluminum is lower than that of Al-CupMg LY12 under the same experimental condition. The most heat energy is absorbed by the solution in the process of microarc oxidation.