ER70s-6焊丝钢洁净度和表面质量研究

Cleanness and Surface Quality Research of ER70s-6 Weld Wire Steel

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 王剑斌李京社杨树峰黄运华胡道锋李翔

【Author】 Wang Jian-bin1,LI Jing-she1,YANG Shu-feng1,HUANG Yun-hua1,HU Dao-feng2,LI Xiang2(1.Metallurgical and Ecological Engineering School,University of Science and Technology Beijing,Beijing 100083,China;2.Second Steel Plant of Nanjing Iron and Steel Corporation,Nianjing 210035,Jiangshu,China)

【机构】 北京科技大学冶金与生态工程学院南京钢铁集团公司第二炼钢厂南京钢铁集团公司第二炼钢厂 北京100083北京100083江苏南京210035

【摘要】 钢的洁净度和铸坯的表面缺陷直接影响焊丝钢的性能。分析了炼钢各工序钢液中的全氧和夹杂物数量、夹杂物成分和形貌;统计了铸坯的表面缺陷。其结果表明,钢中夹杂物主要有以MnO-Al2O3-SiO2-CaO为主的复合脱氧氧化物夹杂物、MnO-Al2O3脱氧产物夹杂,铸坯表面缺陷主要有表面气孔和表面裂纹。

【Abstract】 The purity of steel has direct effect on its mechanical properties.the oxygen content、inclusion quantity、the component of inclusion and the inclusion appearance were analyzed,and also the surface flaw was counted.The result shows that the main type of inclusions in the ER70s-6 weld wire steel is complex oxide system,including MnO-Al2O3-SiO2-CaO system,MnO-SiO2 system and there are two surface flaw on the continuous cast slab,one is surface pores,the other is surface crack.

【关键词】 焊丝钢钢包非金属夹杂物
【Key words】 weld wire steelladle furnacenon-metallic inclusion