含碳球团的还原性和还原冷却后的强度

Reduction and Strength after Reduction of Cooled Pellet Contain Carbon

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 吴铿齐渊洪赵继伟冯根生杜春荣

【Author】 WU Keng ZHAO Jiwei; FENG Gensheng ; DU Chunrong Metallurgy School, UST Beijing, Beijing 100083, QI Yuanhong Central iron and Steel institute, Beijing 100081

【机构】 北京科技大学冶金学院!北京100083北京钢铁研究总院!北京100081

【摘要】 在 1273~1573 K条件下研究了不同煤种、木炭和石墨与不同种类矿石制成含碳球团 的还原速度;进而讨论了温度、配碳比(C/O)、挥发分含量等因素对含碳球团还原所需时间和 金属化率的影响.通过测定含碳球团还原冷却后的强度,对影响强度因素进行了分析.还原冷 却后的强度在温度 1273 K时较低,配入含挥发分较高的气煤,可以使还原冷却后的强度提高, 加快反应速度.

【Abstract】 The reduction experiment of the pellets containing carbon, which consist of different kinds of iron ore and coal (including graphite and charcoal), was carbon out. The effect of temperature, rate of carbon and volatility etc. on the reduction time and metallization of the pellets has been discussed. The strength of the reduced and cooled pellets was measured and the influence of the factors was analysed. The strength of pellets at temperature 1 273 K is low. When the gas coal of high volatility is added, the pellet is becoming to be reduced quickly and its strength is increased.

【基金】 国家“攀登计划”重点项目
  • 【文献出处】 北京科技大学学报 ,JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING , 编辑部邮箱 ,2000年02期
  • 【分类号】TF046
  • 【被引频次】17
  • 【下载频次】470
节点文献中: 

本文链接的文献网络图示:

本文的引文网络