节点文献

中轧车间大规格圆钢表面麻坑产生原因分析

Cause Analysis on Produced Scalemark on the Face of Big Size Round Steel in Medium Section Rolling Workshop

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 韩兴军; 张继奎; 李修峰; 翟正龙;

【Author】 Han Xingjun,Zhang Jikui,Li Xiufeng,Zhai Zhenglong (The Technique Development Centor of Laiwu Iron and Steel Group Co.,Ltd.)

【机构】 莱芜钢铁集团有限公司技术开发中心;

【摘要】 针对莱钢特钢厂中轧车间大规格圆钢(65~85m m )所出现的表面麻坑的成因进行分析,发现钢坯在加热炉中生成的氧化铁皮在轧制过程中未能脱净是表面麻坑产生的主要原因。为此提出了改善烧嘴控制、降低炉内氧化性气氛、钢坯出炉轧制前翻钢90°等有效措施。

【Abstract】 Through cause analysis to produced scalemark on the face of big size round steel(65~85mm) in medium section rolling workshop of special steel plant of Laiwu iron and steel group Co.,Ltd.,it is discovered that the main cause produced scale mark on the face of big size round steel is having scale on the rolled billet face which is heated in heating furnace.For overcoming this defect,the some effective measures consisted of improving the burner control of heating furnace,decreasing the oxidizing atmosphere in heating furnace and turning the billet for 90 degree before it is out of the furnace and rolled are puted forward.

【关键词】 圆钢; 过烧; 氧化铁皮; 表面缺陷;
【Key words】 round steel; overburns; scale; face defect;
  • 【文献出处】 山东冶金 ,SHANDONG METALLURGY , 编辑部邮箱 ,1999年05期
  • 【分类号】TG335.6
  • 【被引频次】4