【摘要】 用电阻加热引上法生长了不开裂、全透明的具有倍频性能的铌酸钾锂(KLN)晶体。研究了影响晶体开裂的主要因素和晶体生长的稳定性。发现用引上法生长KLN晶体时,要得到全透明、不开裂的KLN晶体,熔体中Li2O的含量应该低于26.5mol%,拉速应低于0.5mm/h,以及生长过程中应该选择凸的固液界面以保证晶体生长的稳定性。在Li2O含量较高的熔体中生长KLN晶体时,[100]取向的籽晶比[001]取向的籽晶更有利于晶体生长。用由Li2O含量为26mol%的熔体中沿[100]取向生长的KLN晶体对Ti∶Al2O3激光器输出的820nm的激光倍频,获得410nm的蓝光输出
【Abstract】 The crack free and full transparent potassium lithium niobate (KLN) crystals with frequency doubling performance have been grown by means of the resistance heating Czochralski (CZ) technique.The influence factors of crystal cracking and the stability of crystal growth have been studied.In order to obtain the crack free and full transparent KLN crystals by the CZ technique,the Li 2O content in melt should be less than 26.5mol% and the pulling rate should be lower than 0.5mm/h as well as selecting a axis seed was necessary.And also it was necessary to keep convex shape of solid liquid interface for the stability of the crystal growth.We have realized the blue light output at 410nm by doubling the 820nm light wave generated from Ti∶sapphire laser.
【Key words】 ferroelectric crystal; crystal pulling; frequency doubling; potassium lithium niobate crystal; ferroelectric domain; nonlinear optical crystal;
- 【文献出处】 人工晶体学报 ,JOURNAL OF SYNTHETIC CRYSTALS , 编辑部邮箱 ,1999年02期
- 【分类号】O782
- 【被引频次】4
- 【下载频次】87