聚乙烯醇基中空活性炭纤维的制备——碳化过程的研究
PREPARATION OF POLYVINYLALCOHOL BASED HOLLOW ACF ——STUDY ON CARBONIZATION PROCESS
【摘要】 讨论了用聚乙烯醇纤维制备活性炭纤维的碳化过程中,纤维成分、结晶形态及物理织构的变化,并指出了中空结构的形成过程和影响因素。获得较高得率的均匀活性炭纤维,应采用7℃/m in 较慢的升温速率。
【Abstract】 The changes in fiber component, crystalline morphology and physical fabric structure during the course of carbonization of polyvinylalcohol fiber that was used to prepare activated carbon fiber were discussed. The formation of the hollow structure and the influence factors were pointed out. In order to get the higher yield of uniform ACF, the temperature rising rate should be given as 7℃/min.
【关键词】 聚乙烯醇;
活性炭纤维;
制备;
碳化;
【Key words】 polyvinylalcohol; activated carbon fiber; preparation; carbonization;
【Key words】 polyvinylalcohol; activated carbon fiber; preparation; carbonization;
- 【文献出处】 合成纤维工业 ,CHINA SYNTHETIC FIBER INDUSTRY , 编辑部邮箱 ,1999年05期
- 【分类号】TQ342
- 【被引频次】6
- 【下载频次】625