节点文献

风扇磨煤机ZGMn13冲击板的失效分析

FAILURE ANSLYSIS OF ZGMn13 FAN BLADE IN COAL CRASHERS

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 刘白曲敬信郝诗明

【Author】 LIU Bai,QU Jin-xin,HAO Shi-ming(Material Science and Engineering Dept of China University of Mining and Technology,Beijin 100083,China Mechnical Eng. Dept. of Changsha University,Changsha 410003,China)

【机构】 中国矿业大学材料科学与工程系长沙大学机械工程系

【摘要】 ZGMn13冲击板的失效方式为不同角度的粒子撞击和冲刷,其表面可以分为三个典型的磨损区域:低角度撞击区、高角度撞击区和冲刷区。详细分析了该三个磨损区域的磨损机理。对次表面分析的结果表明,在低角度撞击和冲刷条件下,高锰钢未能充分加工硬化,耐磨性提高有限。

【Abstract】 The granule impact in different angle and abrasion were main failure pattern with ZGMn13 fan blades on which was divided into three typical wear Zones: Low-angle impact Zone,High-angle impact Zone and abrasion Zone.The wear mechanism in each Zone was analysed detailly.The Sub-surface analysis showed that in condition of low-angle impact and abrasion the fan blades of ZGMn13 Were not hardening by deformation fully So that its wearproof ability increase finitely.

【关键词】 ZGMn13冲击板冲蚀磨损
【Key words】 ZGMn13Fan bladeAbrasion
  • 【会议录名称】 全国材料理化测试与产品质量控制学术研讨会论文专辑(物理测试部分)
  • 【会议名称】全国材料理化测试与产品质量控制学术研讨会
  • 【会议时间】2002-11
  • 【分类号】TD453
  • 【主办单位】中国机械工程学会理化检验分会、《理化检验》杂志社、上海材料研究所