【摘要】 利用静电自组装法,将羧甲基纤维素(CMC)组装到Fe3O4上得到Fe3O4@CMC,再通过自由基聚合反应将丙烯酸(AA)和丙烯酰胺(A M)接枝交联到Fe3O4@C M C上,制备出Fe3O4@CMC-g-p(AA-co-AM)(Fe3O4@hydrogel)微球。利用TEM、XRD、FTIR、TGA、XPS、BET等技术对Fe3O4hydrogel微球进行了表征,并将其作为催化剂应用于类芬顿高级氧化反应中催化降解酸性红73。结果表明:Fe3O4@hydrogel仍为反尖晶石型结构,共聚物CMC-g-p(AA-co-AM)成功包覆在Fe3O4表面,且含量为17.7%,复合微球平均粒径在10nm左右,饱和磁化强度为44.8emu/g,BET表面积为73.5m2/g,平均孔直径为8.3nm,为介孔结构。Fe3O4@hydrogel微球对酸性染料废水有良好的催化降解性能,通过调节芬顿反应体系中初始p H值、催化剂用量以及H2O2浓度,得到反应最适条件为p H3.5、H2O210m m ol/l、催化剂用量200mg/l。在此条件下3h内能达到对酸性红7399.83%以上的降解。
【Abstract】 Fe3O4@CMC-g-p(A A-co-A M)(Fe3O4@hyd rogel) microspheres were prepared by electrostatic self-assembly method and radical polymerization reaction. The as-prepared microspheres were characterized by TEM, XRD, FTIR, TGA, XPS and BET techniques. Fe3O4@hydrogels were used for degradation of Acid Red 73(AR73) through Fenton advanced oxidation reaction. It was found that Fe3O4@hydrogel was still anti-spinel structure and copolymer CMC-g-p(AA-co-AM) was successfully coated on Fe3O4 surface. The content of hydrogel in the particles was 17.7%. The average diameters of the composite microspheres was about 10 nm. The saturation magnetization intensity was 44.8 emu/g, the BET surface area was 73.5 m2/g. Fe3O4@hydrogel microspheres exhibited excellent catalytic degradation performance for acidic dye wastewater. The optimal reaction conditions were initial solution p H of 3.5, H2O2 of 10 mmol/L and catalyst dosage of 200 mg/l. Under this condition, up to 99.83% of the AR73 can be degraded within 3 h.
【Key words】 Fe3O4; hydrogel; fenton-like reaction; catalytic degradation; acidic wastewater;
- 【文献出处】 中华纸业 ,China Pulp & Paper Industry , 编辑部邮箱 ,2020年04期
- 【分类号】X703
- 【下载频次】208