【摘要】 CuO added Pb0.92Sr0.06Ba0.02(Mg1/3Nb2/3)0.25(Ti0.53Zr0.47)0.75O3 ceramics were studied to prepare high-quality multilayer piezoelectric actuators with pure Ag electrodes at 900℃. Cu O addition not only reduced the sintering temperature significantly from 1260℃ to 900℃ but also improved the ceramic density to 7.742 g/cm3. The 0.7 wt.% Cu O added ceramic sintered at 900℃ shows the remnant polarization(Pr) of 40 μC/cm2, 0.28% strain at 40 kV/cm, and the piezoelectric coefficient(d33) of 630 pC/N. This ceramic shows a strong relaxor characteristic with a Curie temperature of 200℃. Furthermore, the 0.7 wt.% CuO added ceramic and pure Ag electrodes were co-fired at 900℃ to prepare a high-quality multilayer piezoelectric actuator with a d33 of over 450 pC/N per ceramic layer.

【Abstract】 CuO added Pb0.92Sr0.06Ba0.02(Mg1/3Nb2/3)0.25(Ti0.53Zr0.47)0.75O3 ceramics were studied to prepare high-quality multilayer piezoelectric actuators with pure Ag electrodes at 900℃. Cu O addition not only reduced the sintering temperature significantly from 1260℃ to 900℃ but also improved the ceramic density to 7.742 g/cm3. The 0.7 wt.% Cu O added ceramic sintered at 900℃ shows the remnant polarization(Pr) of 40 μC/cm2, 0.28% strain at 40 kV/cm, and the piezoelectric coefficient(d33) of 630 pC/N. This ceramic shows a strong relaxor characteristic with a Curie temperature of 200℃. Furthermore, the 0.7 wt.% CuO added ceramic and pure Ag electrodes were co-fired at 900℃ to prepare a high-quality multilayer piezoelectric actuator with a d33 of over 450 pC/N per ceramic layer.

【基金】 Project supported by the National Natural Science Foundation of China(Grant Nos.51472118,51602156,52177072,and 11274174);the Fundamental Research Funds for the Central Universities,China(Grant Nos.30916011104 and 30916011208)
  • 【文献出处】 Chinese Physics B ,中国物理B , 编辑部邮箱 ,2017年03期
  • 【分类号】TN384
  • 【被引频次】1
  • 【下载频次】31
节点文献中: 

本文链接的文献网络图示:

本文的引文网络