陕西某金矿选矿试验研究
Experimental research on mineral processing for a gold ore in Shaanxi Province
【摘要】 陕西某金矿石中金以微细粒浸染状分布在黄铁矿、毒砂及脉石矿物中,40.53%以单体和连生金形式存在,硫化物中金占33.04%,脉石中金占26.43%,直接氰化浸出效率极低,金的浸出率仅为43.83%.为实现该金矿资源的有效回收,根据该矿石性质,对比"原矿氰化浸出"进行了"原矿浮选—浮选精矿氰化浸出"以及"原矿浮选—浮选精矿焙烧—焙砂氰化工艺"3种工艺试验。试验结果表明,"原矿浮选—浮选精矿焙烧—焙砂氰化"的工艺可明显提高金的浸出率,金的浸出率可提高到69.24%,是处理该矿石的最佳方案。
【Abstract】 The gold occurred as fine and dissemination in pyrite,arsenopyrite and gangue minerals in a gold ore in Shaanxi province. The gold occurred as crystal grain and under-liberated particles accounted for 40. 53%; gold-bearing pyrite accounted for 33. 04% and other 26. 43% gold existed in the gangue minerals. The leaching rate of gold was very low if the process of cyanide leaching of crude mineral ores was adopted and the leaching rate was only 43. 83%. Based on the ore properties,the flotation for crude mineral ores-cyanide leaching of flotation concentrate,and flotation for crude mineral ores-roasting for flotation concentrate-cyanide leaching for calcining were researched,and the results indicate the most suitable process for this gold ore is flotation for crude mineral ores-roasting for flotation concentrate-cyanide leaching for calcining,and an leaching rate of 69. 24% has been reached.
- 【文献出处】 西安科技大学学报 ,Journal of Xi’an University of Science and Technology , 编辑部邮箱 ,2017年01期
- 【分类号】TD953
- 【被引频次】6
- 【下载频次】106