In our previous experiment on CR-39 detectors,we found out that bulk etch rate of irradiated area is different from unirradiated area.Therefore,the traditional etching model should be revised.In this case,our modification which based on the theoretical studies printing out and the AFM observation was put forward and new etch rate:V′=Vt/Virr was defined.Then,modified track-diameter kinetics was used to clarify AFM analysis.In this research,the key parameters for 100MeV Silicon ion include Vt=4.12μm/h,Virr=2....
【更新日期】
2011-11-04
【分类号】
O572.21
【正文快照】