节点文献
一种新型可切削生物活性微晶玻璃的生物安全性评价
Biological safety assessment of a new machinable bioactive glass-ceramic
【摘要】 背景:自主设计的可切削生物活性微晶玻璃,在保证抗弯强度的同时,有效降低了熔制温度、制备成本。在临床应用前,除必要的机械、理化性能研究外,还需进行生物相容性评估。目的:观察新型可切削生物活性微晶玻璃对小鼠有无全身毒性作用,评价其生物安全性。方法:将纯系昆明种小鼠随机分为实验组、阴性对照组和阳性对照组,实验组经口灌注可切削生物活性微晶玻璃的阿拉伯胶混悬液,阴性对照组灌注等体积阿拉伯胶,阳性对照组灌注醋酸铅溶液,于灌注后24,48,72h观察小鼠一般状态、毒性表现并记录体质量变化。最后处死小鼠取出肝、肾,做光、电镜检查。结果与结论:72h内,实验组小鼠体质量未下降,与阴性对照组比较,差异无显著性意义(P>0.05),肝、肾组织未见病理改变。提示该新型可切削生物活性微晶玻璃经短期口服后对机体无全身毒性。
【Abstract】 BACKGROUND:The machinable bioactive glass-ceramic we designed recently have a lower melting temperature,and preparation of cost while bending strength in ensuring the same time.Prior to clinical application,biocompatibility should be evaluated.OBJECTIVE:To observe the new machinable bioactive glass-ceramics on the availability of systemic toxicity in mice and evaluate its biological security.METHODS:The Kunming mice were randomly divided into an experimental group,negative control group and positive control group.Mice in experimental group were orally perfused with the suspension of machinable bioactive glass-ceramics and Arabic gum.While the mice in the negative control group were treated with an equal volume of Arabic gum,and the mice in the positive control group were treated with an equal volume of lead acetate solution.The general state and toxicity of mice were observed and body mass was recorded after 24 hours,48 hours,and 72 hours.Finally the mice were sacrificed,and the morphological changes in liver and kidney were then examined by light and electron microscopy.RESULTS AND CONCLUSION:The body mass of mice in the experimental group was not decreased significantly compared with the mice in the negative control group in 72 hours(P > 0.05).Pathological changes of liver and kidney in the experimental group did not be found.The new machinable bioactive glass-ceramic did not show systemic toxicity for a short term.
- 【文献出处】 中国组织工程研究与临床康复 ,Journal of Clinical Rehabilitative Tissue Engineering Research , 编辑部邮箱 ,2010年12期
- 【分类号】R318.08
- 【下载频次】144