溶液一步法制备氧化锌纳米棒
Preparation of ZnO Nanorods by One-step Solution Growth Method
【摘要】 以氯化锌(ZnC l2)、氢氧化钠(NaOH)为原料,分别以十二烷基磺酸钠(SDS)和十六烷基三甲基溴化铵(CTAB)为表面活性剂,采用溶液一步法合成了氧化锌(ZnO)纳米棒。结果表明,合成的ZnO纳米棒直径为20~40nm,长度达150nm~2μm。
【Abstract】 The ZnO nanorods were prepared through one-step solution growth method by using ZnCl2 and NaOH as raw materials,and taking sodium dodecyl sulfonate(SDS) and hexadecyl trimethyl ammonium bromide(CTAB) as sulface active agents.Results showed that the diameter of synthetized ZnO nanorods is in the range of 20~40nm,and the length of the ZnO nanorods is up to 150nm~2μm.