【摘要】 用100 t EAF-LF(VD)-300 mm×320 mm连铸-连轧工艺生产的48MnV钢(%:0.45~0.51 C、0.90~1.20Mn、0.05~0.10V)出现粗大晶粒,经13道次轧成的125 mm×125 mm方钢(0.030%~0.050%Ti)的晶粒度为3~4级,经9道次轧成的Φ141 mm圆钢(0.030%~0.053%Ti)的晶粒度为4~5级;但通过加0.018%~0.035%Ti和0.021%~0.029%Nb后,经9道次轧制的Φ141 mm圆钢的晶粒度达5.5~6.5级,显著提高钢的强韧性。

【Abstract】 Coarse grains occurred in the non-quenched-tempered steel 48MnV(%:0.45~0.51C,0.90~1.20Mn, 0.05~0.10V) produced by 100 t EAF-LF(VD)-300 mm×320 mm casting-continuous rolling process.As added 0.030%~0.050%Ti in steel,the rating of grain in 125 mm×125 mm square bar rolled with 13 passes was 3~4;the rating of grain inΦ141 mm round bar(contained 0.030%~0.053%Ti) rolled with 9 passes was 4~5;but as added 0.018%~0.035%Ti and 0.021%~0.029%Nb in steel,the rating of grain inΦ141 mm round bar rolled with 9 passes was 5.5~6.5 in order to obviously increase strength and toughness of steel.

  • 【分类号】TF76
  • 【被引频次】3
  • 【下载频次】188
节点文献中: 

本文链接的文献网络图示:

本文的引文网络