节点文献

含铟锌精矿低温氧压酸浸液铟的回收试验研究

Study on Recovering Indium from the Oxygen Pressure-Leaching Solution of Indium-Containing Zinc Concentrate

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 王振文尹飞江培海王成彦

【Author】 WANG Zhen-wen,YIN Fei,JANG Pei-hai,WANG Cheng-yan(Beijing General Research Institute of Mining and Metallurgy,Beijing 100044,China)

【机构】 北京矿冶研究总院

【摘要】 以含铟锌精矿氧压酸浸液为原料,利用锌精矿还原Fe3+、中和沉铟方法进行铟的富集。在95℃、锌精矿加入量为理论量3倍、还原120 min条件下,Fe3+的还原率达到96%;中和沉铟时控制终点pH=4.0、温度70℃、时间60 min、通入氮气作为保护气条件下,沉铟后液含铟仅为0.004 g/L,所得铟渣品位在1%左右,铟铁比在8.3左右,铟得到很好的富集。

【Abstract】 By using the zinc concentrate leaching solution with indium contained as raw material,the precess of riching indium was studied by method of reducing Fe3+ by using the zinc concentrate and neutralizing-prcipitation indium.The results showed that the reducing rate of Fe3+ was 96% for 120 minutes of reduceing time at 95℃ with adding quantity of the zinc concentrate 3 times as the theorrtical need;consistency of indium in liquid after precipitating indium was only 0.004 g/L,the content of indium in precipitate was around 1%,the quality rate of indium to iron in precipitate is about 8.3.

【关键词】 锌精矿还原中和
【Key words】 Zinc concentrateReducingNeutralizationIndium
  • 【文献出处】 有色金属(冶炼部分) ,Nonferrous Metals(Extractive Metallurgy) , 编辑部邮箱 ,2009年06期