节点文献
镁合金微弧氧化着色膜研究
Study on the Coloring Coating by Micro-arc Oxidation on Magnesium Alloys
【摘要】 镁合金在电子工业中的快速发展对装饰性能提出了更高的要求。主要研究了如何在微弧氧化的同时进行氧化着色。膜层制备选取的基材为AZ91,电解溶液由硅酸盐为主的碱性溶液组成,配方为:Na2SiO3 5~30g/L,KMnO4 1~20g/L,NaOH 1~5g/L,KF 5~8g/L,Na3C6H5O7 0.5~2g/L,EDTA 0.5~2g/L。在电解液中添加着色盐KMnO4,形成了颜色各异的黄色陶瓷膜层。研究发现,膜层呈现出黄色主要是由于在膜层中生成了Mg6MnO8相,该物相在氧化膜中含量不同和分布差异将导致样品颜色深浅不同。
【Abstract】 With the rapid development of magnesium alloys in electric industry,the more advanced requirement of decorative property is given.How to color is studied during the process of micro-arc oxidation.Micro-arc oxidation ceramic(MAO) coating on AZ91 magnesium alloy is prepared in a silicate alkalinous solution(Na2SiO3 5~30g/L, KMnO4 1~20g/L,NaOH 1~5g/L,KF 5~8g/L,Na3C6H5O7 0.5~2g/L,EDTA 0.5~2g/L).By adding KMnO4 into the silicate alkalinous solution the coatings can take on all sorts of yellow effects.The results show that MAO coatings take on yellow effect depending on the phase of Mg6MnO8.The difference of Mg6 MnO8 content or distribution can lead to the difference of yellow depth.
【Key words】 magnesium alloys; micro-arc oxidation(MAO); oxidizing and coloring; Mg6MnO8; coating;
- 【文献出处】 材料导报 ,Materials Review , 编辑部邮箱 ,2009年S1期
- 【分类号】TG174.4
- 【被引频次】12