撞击流反应制备纳米磷酸锌改进工艺研究
Improvement on Producing Process of Preparing Nano-zinc Phosphate by Impinging Stream Reaction
【摘要】 在浸没循环撞击流反应器(SCISR)中,以工业氧化锌和磷酸为原料,采用液-液相反应-沉淀法制备纳米磷酸锌。实验产品进行了X射线衍射(XRD)和电子透射显微镜(TEM)表征。探讨了反应物浓度、反应温度、反应时间及原料配比对收率的影响;初步确定制备纳米磷酸锌较适宜的工艺条件为:氧化锌溶液浓度0.86 mol/L,反应温度70℃,反应时间1 h,磷酸与氧化锌摩尔比0.67。XRD和TEM表征表明产品主要成分为Zn3(PO4)2.2H2O,平均粒径30—50nm。
【Abstract】 Nano-zinc phosphate was prepared by liquid-liquid reaction-precipitation in the submerged circulating impinging stream reactor(SCISR) with commercial zinc oxide and phosphoric acid as the raw materials.The products were characterized by XRD and TEM.The influences of reactant concentration,reaction temperature,reaction time,and formula of the reactants on the yield were investigated,and the more appropriate conditions for preparation of nano-zinc phosphate were determined primarily as follows: ZnO concentration 0.86 mol/L,reaction temperature 70 ℃,reaction time 1 h,and the mole ratio of H3PO4/ZnO 0.67.The results of determination with XRD and TEM show that the major component in the product is Zn3(PO4)2·2H2O,and the average size of particles in the product is ranged 30 nm to 50 nm.
【Key words】 impinging stream; nano-preparation; zinc phosphate; reaction-precipitation;
- 【文献出处】 武汉理工大学学报 ,Journal of Wuhan University of Technology , 编辑部邮箱 ,2008年09期
- 【分类号】TB383.1
- 【被引频次】7
- 【下载频次】169