【摘要】 采用三聚氰胺甲醛树脂辊压浸注桦木单板,通过热压定型得到树脂增强重组材。探讨不同树脂固体含量、辊压压榨率和热压压力对板材吸水厚度膨胀率、静曲强度、顺纹抗拉强度、胶合强度等性能的影响。结果表明,树脂固体含量50%、辊压压榨率20%、热压压力2.0 MPa时,重组材的物理力学性能指标综合水平较佳。

【Abstract】 To improve the performance of veneer-based panel products,melamine-formaldehyde resin was impregnated into each individual Birch veneer by roller-pressing before lamination.The effects of resin content,compression rate of the roller-pressing,and pressure during hot-pressing were evaluated for selected panel properties including thickness swell,modulus of rupture,tensile strength,and internal bond strength.The results showed that with 50% resin content,20% compression ratio,and 2.0 MPa pressure during hot pressing to make the reconstituted veneer lumber,performance of the lumber could meet the desirable specifications.

【基金】 “十一五”国家科技支撑计划专题(2006BAD18B06);引进国际先进林业科学技术计划“948”专题(2006-4-C04)
  • 【文献出处】 木材工业 ,China Wood Industry , 编辑部邮箱 ,2008年03期
  • 【分类号】TS653
  • 【被引频次】4
  • 【下载频次】91
节点文献中: 

本文链接的文献网络图示:

本文的引文网络