节点文献

GCr15轴承钢LF精炼过程钢的洁净度变化

Change in cleanliness of GCr15 bearing steel in LF refining

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 张树海邢梅峦郝彦英孙玉春

【Author】 ZHANG Shu-hai1,XING Mei-luan2,HAO Yan-ying2,SUN Yu-chun2(1.Hebei Vocational Institute of Industry and Technology,Shijiazhuang 050091,China;2.Shijiazhuang Iron and Steel Co.,ltd,Shijiazhuang 050031,China)

【机构】 河北工业职业技术学院石家庄钢铁有限责任公司

【摘要】 对GCr15轴承钢LF精炼过程各阶段的钢中氧及夹杂物含量进行了研究。结果表明,在现有工艺条件下,LF精炼15~20min时钢中氧含量已降低到较低水平,LF精炼结束后软吹时间控制15min左右较为合理;LF精炼结束及中间包钢中大部分夹杂物尺寸在15μm以下;应进一步加强浇铸环节的控制,减少钢水的二次污染。

【Abstract】 This paper investigates the oxygen content and non-metal inclusions of the GCr15 bearing steel in each and every phase of the LF refining process.The results indicate that in the existing process conditions the oxygen content of steel has been reduced to a lower level through 15 to 20 minutes of LF refining.The appropriate time for soft blowing upon completion of LF refining is proved to be about 15 minutes.The dimension of the non-metal inclusions at the end of LF process is below 15μm;To reduce the secondary contamination of steel the casting process should be strengthened.

【关键词】 GCr15轴承钢LF氧含量非金属夹杂物
【Key words】 GCr15 bearing steelLFoxygen contentnonmetal inclusion
  • 【分类号】TF769
  • 【被引频次】2
  • 【下载频次】333
节点文献中: 

本文链接的文献网络图示:

本文的引文网络