醇—水溶液共沉淀法制备铬锡红陶瓷色料超细粉
SYNTHESIS OF ULTRA FINE CHROME-TIN PINK PIGMENT BY COPRECIPITATION METHOD OF ALOHOL-AQUEOUS SALT SOLUTIONS
【摘要】 采用醇—水溶液共沉淀法制备铬锡红色料。通过选择适当的分散剂,可制得颗粒大小在0.5-1滋m、团聚少的超细铬锡红色料。与通常的水溶剂共沉淀法相比,样品颗粒更细,粒度分布范围更窄,呈色更鲜艳,煅烧温度更低。
【Abstract】 A novel methed which involved coprecipitation with an alcohol-water mixture as a solvent was used to synthesize the ultra fine Cr-Sn pink pigment. By adding appropriato dispersant ,weakly agglomerated powders of Cr-Sn pink with average particle size of 0.5~1mm can be obtained .Contrast with the ordinary trend of the powder synthesized by hydrosolvent coprecipitation , better colour? smaller grain?narrower grain distribution and lower synthesis temperature of the sample.
【关键词】 铬锡红色料;
醇—水溶液共沉淀;
超细粉;
【Key words】 Cr-Sn pink; Alcohol-Water mixture solvent; Coprecipitation methed; Ultramicro; powder;
【Key words】 Cr-Sn pink; Alcohol-Water mixture solvent; Coprecipitation methed; Ultramicro; powder;
【基金】 山东大学胶体与界面化学教育部重点实验室资助
- 【文献出处】 中国陶瓷工业 ,China Ceramic Industry , 编辑部邮箱 ,2004年04期
- 【分类号】TQ174.45
- 【被引频次】7
- 【下载频次】235