【作者】 代书华刘百臣赵庆杰沈峰满余艾冰

【Author】 DAI Shu-hua~1, LIU Bai-chen~1, ZHAO Qing-jie~1, SHEN Feng-man~1, YU Ai-bing~2 (1.School of Materials and Metallurgy ,Northeastern University,Shenyang,110004,China;2.School of Material Science and Engineering, University of New South Wales, Sydney NSW2052, Australia)

【机构】 东北大学材料与冶金学院新南威尔士大学材料科学与工程学院 辽宁沈阳110004辽宁沈阳110004澳大利亚悉尼NSW2052

【摘要】 为了充分利用某钢铁公司含锌电炉粉尘中的锌、铁及碳等有价元素,在实验室条件下考察了水分、造球时间、内配煤量对生球强度的影响以期获得最佳工艺参数,并为球团用于工业生产提供基本数据.试验结果表明适宜的水分为8 4%~10%,适宜的造球时间为30min,内配煤量对生球强度影响很小.

【Abstract】 Aiming at the utilization of zinc, iron and carbon in EAF dust,the influences of water addition,pelletizing time and coal addition on strength of the green pellet are studied under laboratory conditions. And the influences of these factors on strength of the green pellet are investigated to obtain the optimum pelletizing parameters and provide basic data for the development of industrial pelletizing process. The experimental results show that the proper pelletizing parameters are 8.4%~10% of water addition and 30 minutes of pelletizing time. The coal addition has little influence on strength of green pellets.

【基金】 国家杰出青年基金项目(50228405).
  • 【文献出处】 材料与冶金学报 ,Journal of Materials and Metallurgy , 编辑部邮箱 ,2004年03期
  • 【分类号】X757;TF805.2
  • 【被引频次】8
  • 【下载频次】247