节点文献
挤压铸造高速钢轧辊的研制和应用
The study on extrusion casting high speed steel roll
【摘要】 挤压铸造的压力、保压时间和压下速度是影响高速钢轧辊缩孔的重要因素。采用浇注温度 14 0 0 14 5 0℃、压力15 0MPa、保压时间 12 0 15 0s ,压下速度 14 16mm/s ,可获得组织致密、无偏析、加工量少的高速钢轧辊。
【Abstract】 The effects of extrusion casting process on the properties of HSS roll are researched,pressure,pressing time and pressing speed are three important factors affecting shrinkage cavity,as pouring temperature is 1400~1450℃,pressure is 150MPa,pressing time is 120~150s,pressing speed is 14~16mm/s,HSS roll having compact structure,no segregation and small working allowance is obtained .
- 【文献出处】 现代制造工程 ,Machinery Manufacturing Engineer , 编辑部邮箱 ,2003年06期
- 【分类号】TG333.17
- 【被引频次】3
- 【下载频次】95