节点文献

等离子喷涂生物活性梯度涂层的残余应力与结合强度

Residual Stress and Bond Strength of Bioactive Gradient Coatings Plasma-sprayed

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 王迎军宁成云陈楷赵子衷李尚周马利泰冯景伟黄瑞福

【Author】 WANG Ying-Jun; NING Cheng-Yun; CHEN Kai; ZHAO Zi-Zhong; LI Shang-Zhou (South China University of Technology Guangzhou 510641 China)MA Li-Tai; FENG Jing-Wei; HUANG Rui-Fu (Shanghai Institute of Ceramics, Chinese Academy of Sciences Shanghai 200050 China)

【机构】 华南理工大学材料学院!广州510641中国科学院上海硅酸盐研究所!上海200050中国科学院上

【摘要】 本研究设计的生物活性梯度涂层材料,通过降低涂层与基体间的热膨胀系数差值,并对喷涂后的涂层材料进行适当热处理,有效地降低了涂层的残余应力,涂层结合强度可达38MPa左右.本实验采用X射线sin2Ψ法对涂层残余应力进行测试,探讨涂层残余应力与结合强度的相互影响关系.

【Abstract】 A material of bioactive gradient coatings was designed. The difference of thermal expansion coefficients between coating and substrate was reduced. The residual stress within the plasmasprayed coatings heat-treated was reduced. The bonding strength of the coatings was measured to be about 38 MPa. The residual stress produced within the coatings was measured by the sin2Ψmethod of XRD, and the influence of residual stress on the bond strength of the coatings was explored.

【基金】 上海硅酸盐研究所高性能陶瓷及超微结构国家重点实验室!9715;广东省自然科学基金!940558
  • 【文献出处】 无机材料学报 ,JOURNAL OF INORGANIC MATERIALS , 编辑部邮箱 ,1998年04期