节点文献
转炉用MgO-C砖和MgO-CaO-C砖蚀损的研究
Comparative study on erosion of Mgo-CaO-C and MgO-C bricks for BOF
【摘要】 研究结果表明:转炉初期渣使MgO-C砖产生结构利落,因而蚀损最严重;但对MgO-CaO-C砖的侵蚀较轻,这是因为在砖的界面上产生了C2S保护层。中期和终期渣对MgO-CaO-C砖的侵蚀由于其更易于被渣中ΣFeO溶解,所以比MgO-C砖要强烈些。
【Abstract】 Erosion of initial slag to MgO-C brick is the worse damage led by structural spalling. But to MgO-CaO-C brick,the damage is not all serious because of a C2S layer formed on the interface of the brick. Erosion of mid and final slagsto MgO-CaO-C brick is stronger than that to MgO-C brick because the former is easily cornded by ΣFeO in the slags.
【关键词】 MeO-C砖;
MgO-CaO-C砖;
侵蚀;
结构剥落;
【Key words】 Magnesia carbon brick; Magnesia calcia carbon brick; Erosion; Structural;
【Key words】 Magnesia carbon brick; Magnesia calcia carbon brick; Erosion; Structural;
- 【文献出处】 耐火材料 ,Refractories , 编辑部邮箱 ,1997年03期
- 【分类号】TQ175
- 【被引频次】1
- 【下载频次】57