节点文献
高表面积活性碳的制备
The New Technique to Prepare High Surface Area Activated Carbon
【摘要】 本文报道了用石油焦、核桃壳为原料,以氢氧化钾为活化剂制备高表积活性碳的新工艺。研究了主要工艺条件对产品性能的影响。结果表明,最佳活化条件为:KOH与原料比为4∶1,活化温度800~900℃。
【Abstract】 In this paper, the new technique to prepare high surface area activated carbon from walnut parting using chemical activation with alkali hydroxides were introduced. The influence of mian processing conditions were studied. Results shown, the optimal condition are as follows:KOH:C=4∶1, activating temperature:800~900℃.
【关键词】 高表面积活性碳;
核桃壳;
氢氧化钾;
【Key words】 High surface area activated carbon; Walnut parting; Potassium hydroxide;
【Key words】 High surface area activated carbon; Walnut parting; Potassium hydroxide;
- 【文献出处】 材料科学与工程 ,MATERIALS SCIENCE AND ENGINEERING , 编辑部邮箱 ,1996年04期
- 【分类号】TQ424.1
- 【被引频次】133
- 【下载频次】864