Investigations on Response Time and Thermal Equilibrium State of Oxygen Probe

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 黄克勤回世强吴卫江刘庆国

【Author】 Huang Keqin; Hui Shiqiang; Wu Weijiang; Liu Qingguo (Department of Physical Chemistry,USTB, Beijing 100083, PRC)

【机构】 北京科技大学物理化学系

【摘要】 本文分别研究了ZrO(MgO)固体电解质管头壁厚、参比电极量对定氧测头响应时间的影响,得出了以ZrO管头壁厚为0.60~0.80mm,Cr/Cr参比电极加入量为40~60mg所组成的定氧测头响应速度最快.同时采用了“双偶法”对定氧测头在工作过程中的热平衡态进行了研究.结果表明:氧浓差电池中的传热是响应过程的控速步骤,氧电势曲线上峰值的产生是起源于电池中的热平衡态.

【Abstract】 Effects of the tip end thickness of ZrO2(MgO) tube and the amount of reference electrode addition on the response time were investigated in this paper. It is concluded that the optimized parameters for tip thickness of ZrO2 (MgO) tube and the amount of reference electrode are 0.60~0.80mm and 40~60mg respectively. The thermal equilibrium of response process for oxygen probe using"Two TC Method" was also investigated. The results show that the heat transfer in the oxygen galvanic cell is the limitting-step in the response process and the peak appeared in the EMF curve is resulted from the thermal equilibrium in the oxygen galvanic cell.

  • 【文献出处】 北京科技大学学报 ,JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING , 编辑部邮箱 ,1994年02期