600℃时球铁珠光体含量与延伸率的关系

The Relationship between Elongation and Pearlitic Content in Ductile Iron at 600℃

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 林汉同; 杨晓红; 熊国庆; 魏伯康;

【Author】 Lin Hantong Yang Xiaohong Xiong Guoqing Wei Bokang

【机构】 华中理工大学机械工程二系; 华中理工大学机械工程二系;

【摘要】 在600℃的条件下,对珠光体球铁试样进行了拉伸试验,得到了珠尤体球铁的动态延伸率和残留延伸率与珠光体含量之间的关系:随珠光体含量的增加,试样的动态延伸率增加,而残留延伸率减小。

【Abstract】 Tensile tests on ductile iron specimens with different pearlitic contents have been carried out at 600℃. Both dynamic elongation and residual elongation have been measured. The results show that with the increase of the pearlitic content, the dynamic elongation of the specimen increases while the residual elongation decreases. It is therefore proposed that both dynamic elongation and residual elongation rather than residual elongation alone be considered as the ductility of ductile iron at elevated temperature (for instance, 600℃).