(GaAl)As/GaAs质子轰击隔离条形DH激光器的退化原因

Causes for degradation of isolated stripe (GaAl) As/GaAs DH lasers by proton bombardment

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 庄婉如; 杨培生; 高季林; 马英棣;

【Author】 Zhuang Wanru, Yang Peisheng, Gao Jilin, Ma Yindi (Institute of Semiconductors, Academia Sinica)

【机构】 中国科学院半导体所; 中国科学院半导体所;

【摘要】 对研制的(GaAl)As/GaAs质子轰击隔离条形DH激光器的退化原因进行了实验分析。结果表明:快退化主要起因于有源区内的暗点、暗线及暗区等缺陷的增殖;腔面氧化是限制寿命在千小时的原因之一;质子轰击引入的点缺陷移入有源区是器件限制寿命在万小时的原因之一。

【Abstract】 We have investigated experimentally the causes for degradation of the isolated stripe CW(GaAl)As/GaAs DH lasers by proton bombardment. The results of ageing tests show that the fast degraded lasers are caused by defects (such as dark spot, dark line and dark region) in the active region extendeing rapidly during the test process. One of the factors limiting the lifetime to 103 hours is the oxidization of the mirror facet of laser cavity; and the moving of mierodefects by proton bombardment into the active region becomes one of the reasons limiting the lifetime to 104 hours.

  • 【文献出处】 中国激光 ,Chinese Journal of Lasers , 编辑部邮箱 ,1983年06期
  • 【被引频次】2
  • 【下载频次】14
节点文献中: 

本文链接的文献网络图示:

本文的引文网络