W和Co对Ni-20Cr基合金高温蠕变行为的影响

INFLUENCE OF W AND Co ON HIGH TEMPERATURE CREEP BEHAVIOUR OF Ni-20Cr BASE ALLOYS

  • 推荐 CAJ下载
  • PDF下载
  • 不支持迅雷等下载工具,请取消加速工具后下载。

【作者】 杨枏森魏育环傅宏镇李文高唐荣德

【Author】 Yang Nansen, Wei Yuhuan, Fu Hongzhen and Zt Wengao (Central Institute of Iron and Steel Research, Ministry of Metallurgical Industry) and Tang Rongde (Pushun Steel Works)

【机构】 冶金工业部钢铁研究总院抚顺钢厂

【摘要】 本文研究了不同W和Co含量的Ni-20Cr基合金的高温稳态蠕变行为。结果表明,W和Co均可提高合金的蠕变激活能Qc,它服从Qc=Ae(kx/lge的关系.Ni-Cr-Co-W合金的稳态蠕变速率(?)s也服从(?)s=Cσmexp(-Qc/RT)的关系。还指出,Ni-Cr-Co-W合金的稳态蠕变速率(?)s与堆垛层错能γ之间,有(?)s ∝γ1.4的关系。

【Abstract】 The steady state creep behaviour of the Ni-20Cr base alloys with various contents of W and Co has been investigated in the temperature range of 940 to 1040℃. Both W and Co may raise the activation energy for creep, Qo, obeyed the relationship:Qc=Aekx/lg? where x is the atomic fraction of W or Co additions; A is a constant for the alloy composition and k is equal to 7.0 and 0.55 for W and Co additions respectively. The steady state creep rate (?)s of Ni-Cr-Co-W alloys was predicated to be:(?)s=Cσm exp (-Qe/RT) where m=6.45±0.10 or 5.3 depending on whether μ phase is present or not. It was also shown that the (?)s varies with the stacking fault energy γ according to the correlation:(?)s∞γ1.4

  • 【文献出处】 金属学报 ,Acta Metallrugica Sinica , 编辑部邮箱 ,1981年01期
  • 【被引频次】9
  • 【下载频次】57
节点文献中: 

本文链接的文献网络图示:

本文的引文网络